Moshkova, M. A., Morozov, P. V., Antipov, A. V., Vakhtomin, Y. B., & Smirnov, K. V. (2021). High-efficiency multi-element superconducting single-photon detector. In I. Prochazka, M. Štefaňák, R. Sobolewski, & A. Gábris (Eds.), Proc. SPIE (Vol. 11771, pp. 2–8). SPIE.
Abstract: We present the result of the creation and investigation of the multi-element superconducting single photon detectors, which can recognize the number of photons (up to six) in a short pulse of the radiation at telecommunication wavelengths range. The best receivers coupled with single-mode fiber have the system quantum efficiency of ⁓85%. The receivers have a 100 ps time resolution and a few nanoseconds dead time that allows them to operate at megahertz counting rate. Implementation of the multi-element architecture for creation of the superconducting single photon detectors with increased sensitive area allows to create the high efficiency receivers coupled with multi-mode fibers and with preserving of the all advantages of superconducting photon counters.
|
Neroev, V. V., Iomdina, E. N., Khandzhyan, A. T., Khodzhabekyan, N. V., Sengaeva, M. D., Ivanova, A. V., et al. (2021). Experimental study of the effect of corneal hydration and its biomechanical properties on the results of photorefractive keratectomy. Vestn. Oftalmol., 137(3), 68–75.
Abstract: Water content in the cornea may affect the outcome of its excimer laser ablation, especially in presbyopic patients with myopic refraction. This hypothesis can be tested by scanning the cornea in the terahertz (THz) range to determine its hydration level.
Purpose: To study the effect of hydration of the cornea determined by non-contact THz scanning and its biomechanical parameters on the results of photorefractive keratectomy (PRK) in an experiment.
Material and methods: PRK was performed using the Nidek EC-5000 QUEST excimer laser on 8 rabbit eyes. Corneal hydration was evaluated by determining the reflection coefficient (RC) in the THz electromagnetic radiation range before PRK, after 3-5 days, and after 1, 2, 3, and 4 months. Clinical examination included autorefractometry, assessment of corneal thickness and other anatomical and optical parameters of the anterior eye segment (Galilei G6, Ziemer Ophthalmic Systems AG 6.0.2, Switzerland), measurement of corneal hysteresis (CH) and corneal resistance factor (CRF) using the Ocular Response Analyzer (ORA; Reichert, USA), as well as tear production (Schirmer test).
Results: The initial water content in the cornea has a significant effect on the thickness of the removed layer, i.e. on the PRK effect, with correlation coefficient of Rs= -0.976 (p<0.01). The correlation between CH and the ablation depth is less pronounced (Rs=0.643), and CRF had no correlation with it (Rs= -0.089). Biomechanical indicators of the cornea depend on its hydration: changes in CH and CRF after excimer laser ablation qualitatively coincide with changes in RC, the correlation coefficient between RC and the initial value of CH is R= -0.619 (moderate negative correlation).
Conclusion: THz scanning is an effective non-contact technology for monitoring corneal hydration level. The mismatch of the hypoeffect of keratorefractive excimer laser intervention planned for patients with presbyopia with the actual outcome can be caused by individual decrease in the initial water content in the cornea.
|
Korneeva, Y. P., Manova, N. N., Dryazgov, M. A., Simonov, N. O., Zolotov, P. I., & Korneev, A. A. (2021). Influence of sheet resistance and strip width on the detection efficiency saturation in micron-wide superconducting strips and large-area meanders. Supercond. Sci. Technol., 34(8), 084001.
Abstract: We report our study of detection efficiency (DE) saturation in wavelength range 400 – 1550 nm for the NbN Superconducting Microstrip Single-Photon Detectors (SMSPD) featuring the strip width up to 3 μm. We observe an expected decrease of the $DE$ saturation plateau with the increase of photon wavelength and decrease of film sheet resistance. At 1.7 K temperature DE saturation can be clearly observed at 1550 nm wavelength in strip with the width up to 2 μm when sheet resistance of the film is above 630Ω/sq. In such strips the length of the saturation plateau almost does not depend on the strip width. We used these films to make meander-shaped detectors with the light sensitive area from 20×20μm2 to a circle 50 μm in diameter. In the latter case, the detector with the strip width of 0.49 μm demonstrates saturation of DE up to 1064 nm wavelength. Although DE at 1310 and 1550 nm is not saturated, it is as high as 60%. The response time is limited by the kinetic inductance and equals to 20 ns(by 1/e decay), timing jitter is 44 ps. When coupled to multi-mode fibre large-area meanders demonstrate significantly higher dark count rate which we attribute to thermal background photons, thus advanced filtering technique would be required for practical applications.
|
Samsonova, A. S., Zolotov, P. I., Baeva, E. M., Lomakin, A. I., Titova, N. A., Kardakova, A. I., et al. (2021). Signatures of surface magnetic disorder in niobium films. IEEE Trans. Appl. Supercond., 31(5), 1–5.
Abstract: We present our studies on the evolution of the normal and superconducting properties with thickness of thin Nb films with a low level of non-magnetic disorder ( kFl≈150 for the thickest film in the set). The analysis of the superconducting behavior points to the presence of magnetic moments, hidden in the native oxide on the surface of Nb films. Using the Abrikosov-Gorkov theory, we obtain the density of surface magnetic moments of 1013 cm −2 , which is in agreement with the previously reported data for Nb films.
|
Korneeva, Y. P., Manova, N. N., Florya, I. N., Mikhailov, M. Y., Dobrovolskiy, O. V., Korneev, A. A., et al. (2020). Different single-photon response of wide and narrow superconducting MoxSi1−x strips. Phys. Rev. Applied, 13(2), 024011 (1 to 7).
Abstract: The photon count rate (PCR) of superconducting single-photon detectors made of MoxSi1−x films shaped as a 2-μm-wide strip and a 115-nm-wide meander strip line is studied experimentally as a function of the dc biasing current at different values of the perpendicular magnetic field. For the wide strip, a crossover current Icross is observed, below which the PCR increases with an increasing magnetic field and above which it decreases. This behavior contrasts with the narrow MoxSi1−x meander, for which no crossover current is observed, thus suggesting different photon-detection mechanisms in the wide and narrow strips. Namely, we argue that in the wide strip the absorbed photon destroys superconductivity locally via the vortex-antivortex mechanism for the emergence of resistance, while in the narrow meander superconductivity is destroyed across the whole strip line, forming a hot belt. Accordingly, the different photon-detection mechanisms associated with vortices and the hot belt determine the qualitative difference in the dependence of the PCR on the magnetic field.
|