Korneeva, Y. P., Vodolazov, D. Y., Semenov, A. V., Florya, I. N., Simonov, N., Baeva, E., et al. (2018). Optical single photon detection in micron-scaled NbN bridges. arXiv:1802.02881v1 [cond-mat.supr-con]. Retrieved August 10, 2024, from https://arxiv.org/abs/1802.02881v1
Abstract: We demonstrate experimentally that single photon detection can be achieved in micron-wide NbN bridges, with widths ranging from 0.53 μm to 5.15 μm and for photon-wavelengths from 408 nm to 1550 nm. The microbridges are biased with a dc current close to the experimental critical current, which is estimated to be about 50 % of the theoretically expected depairing current. These results offer an alternative to the standard superconducting single-photon detectors (SSPDs), based on nanometer scale nanowires implemented in a long meandering structure. The results are consistent with improved theoretical modelling based on the theory of non-equilibrium superconductivity including the vortex-assisted mechanism of initial dissipation.
|
|
|
Sidorova, M. V., Kozorezov, A. G., Semenov, A. V., Korneeva, Y. P., Mikhailov, M. Y., Devizenko, A. Y., et al. (2018). Nonbolometric bottleneck in electron-phonon relaxation in ultrathin WSi films. Phys. Rev. B, 97(18), 184512 (1 to 13).
Abstract: We developed the model of the internal phonon bottleneck to describe the energy exchange between the acoustically soft ultrathin metal film and acoustically rigid substrate. Discriminating phonons in the film into two groups, escaping and nonescaping, we show that electrons and nonescaping phonons may form a unified subsystem, which is cooled down only due to interactions with escaping phonons, either due to direct phonon conversion or indirect sequential interaction with an electronic system. Using an amplitude-modulated absorption of the sub-THz radiation technique, we studied electron-phonon relaxation in ultrathin disordered films of tungsten silicide. We found an experimental proof of the internal phonon bottleneck. The experiment and simulation based on the proposed model agree well, resulting in τe−ph∼140–190 ps at TC=3.4K, supporting the results of earlier measurements by independent techniques.
|
|
|
Sidorova, M. V., Kozorezov, A. G., Semenov, A. V., Korneev, A. A., Chulkova, G. M., Korneeva, Y. P., et al. (2018). Non-bolometric bottleneck in electron-phonon relaxation in ultra-thin WSi film. arXiv:1607.07321v4 [physics.ins-det]. Retrieved August 10, 2024, from https://arxiv.org/abs/1607.07321v4
Abstract: We developed the model of the internal phonon bottleneck to describe the energy exchange between the acoustically soft ultrathin metal film and acoustically rigid substrate. Discriminating phonons in the film into two groups, escaping and nonescaping, we show that electrons and nonescaping phonons may form a unified subsystem, which is cooled down only due to interactions with escaping phonons, either due to direct phonon conversion or indirect sequential interaction with an electronic system. Using an amplitude-modulated absorption of the sub-THz radiation technique, we studied electron-phonon relaxation in ultrathin disordered films of tungsten silicide. We found an experimental proof of the internal phonon bottleneck. The experiment and simulation based on the proposed model agree well, resulting in tau{e-ph} = 140-190 ps at TC = 3.4 K, supporting the results of earlier measurements by independent techniques.
|
|
|
Korneeva, Y., Florya, I., Semenov, A., Korneev, A., & Goltsman, G. (2011). New generation of nanowire NbN superconducting single-photon detector for mid-infrared. IEEE Trans. Appl. Supercond., 21(3), 323–326.
Abstract: We present a break-through approach to mid-infrared single-photon detection based on nanowire NbN superconducting single-photon detectors (SSPD). Although SSPD became a mature technology for telecom wavelengths (1.3-1.55 μm) its further expansion to mid-infrared wavelength was hampered by low sensitivity above 2 μm. We managed to overcome this limit by reducing the nanowire width to 50 nm, while retaining high superconducting properties and connecting the wires in parallel to produce a voltage response of sufficient magnitude. The new device exhibits 10 times better quantum efficiency at 3.5 μm wavelength than the “standard” SSPD.
|
|
|
Korneev, A., Korneeva, Y., Florya, I., Voronov, B., & Goltsman, G. (2012). NbN nanowire superconducting single-photon detector for mid-infrared. Phys. Procedia, 36, 72–76.
Abstract: Superconducting single-photon detectors (SSPD) is typically 100 nm-wide supercondiucting strip in a shape of meander made of 4-nm-thick film. To reduce response time and increase voltage response a parallel connection of the strips was proposed. Recently we demonstrated that reduction of the strip width improves the quantum effciency of such a detector at wavelengths longer than 1.5 μm. Being encourage by this progress in quantum effciency we improved the fabrication process and made parallel-wire SSPD with 40-nm-wide strips covering total area of 10 μm x 10 μm. In this paper we present the results of the characterization of such a parallel-wire SSPD at 10.6 μm wavelength and demonstrate linear dependence of the count rate on the light power as it should be in case of single-photon response.
|
|