Kardakova, A. I., Coumou, P. C. J. J., Finkel, M. I., Morozov, D. V., An, P. P., Goltsman, G. N., et al. (2015). Electron–phonon energy relaxation time in thin strongly disordered titanium nitride films. IEEE Trans. Appl. Supercond., 25(3), 1–4.
Abstract: We have measured the energy relaxation times from the electron bath to the phonon bath in strongly disordered TiN films grown by atomic layer deposition. The measured values of τ eph vary from 12 to 91 ns. Over a temperature range from 3.4 to 1.7 K, they follow T -3 temperature dependence, which are consistent with values of τ eph reported previously for sputtered TiN films. For the most disordered film, with an effective elastic mean free path of 0.35 nm, we find a faster relaxation and a stronger temperature dependence, which may be an additional indication of the influence of strong disorder on a superconductor.
|
|